Description
Firing range: Cone 5-10 (2192º-2372ºF
Bisque temperature: Cone 06 (1855ºF)
Water content: 17%
Plasticity (IP Atterberg): 16
Carbonate content (CaCO3): 0%
Drying shrinkage: 5.5%
Firing shrinkage at Cone 10: 3.9%
Porosity (water absorption) at Cone 10: 2.6%
Dry bending strength: 2.5 N/mm2
Fired bending strength (1300ºC): 37.8 N/mm2
Thermal coefficient (25-500ºC): 59.9×10^-7ºC^-1