Description
Firing range: Cone 6-8 (2269°-2320°F)
Bisque temperature: Cone 06 (1855ºF)
Water content: 26%
Plasticity (IP Atterberg): 11
Carbonate content (CaCO3): 0%
Drying shrinkage: 4.4%
Firing shrinkage at Cone 7: 11.4%
Porosity (water absorption) at Cone 7: 2.8%
Dry bending strength: 4.5 N/mm2
Fired bending strength at Cone 7: 21.0 N/mm2
Thermal coefficient (25-500ºC): 58.8×10-7ºC-1